1. Introduce
– Solid solution strengthening alloys with Ni, Cr, and Fe as the main components
– Alloy can be used in a temperature range from cryogenic to over 1095°C
– Excellent oxidation and heat resistance even at 1095℃
– UNS N06600
* Inconel
- Features
– Resists oxidation and submersion in oxidizing and sulfurizing atmospheres above 900℃
– Non-corrosive to organic and salt solutions
– Excellent mechanical properties such as tensile and yield strength up to about 600℃ - Applications
– High temperature heat resistant equipment(Heat treatment furnace, boiler, jet engine parts, electric heater parts) - Types
– Incoenl 600/601, Inconel 625, Inconel 690, Inconel 718, Inconel 718+, Inconel X-750, etc.
* Inconel 600 vs Inconel 601
– Common points
- nickel-chromium-iron solid solution strengthened alloy
- used for corrosion and heat resistant applications
– Differences
- Features
– Inconel 600 : High strength, good machinability
– Inconel 601 : Good high temperature oxidation resistance - Content
– Inconel 600 has a higher nickel content than Inconel 601
– Inconel 601 has a higher chromium content and a small amount of aluminum added
* UNS
- Abbreviation for Unified Numbering Systems for Metals and Alloys
- Unified unique numbering system for metals and alloys
- A representative number that is compatible with metals and alloys defined in many material-related codes such as ASTM, AISI, ASME, AWS, etc.
* N : Nickel and Nickel Alloys
* UNS N06600 : 06XXX : Chromium(Hastelloy, Nichrome, Inconel and etonite, some with additional element
2. Property
– Good strength, heat resistance, corrosion resistance, oxidation resistance, high temperature oxidation resistance, weldability, creep resistance
| Element | Impact |
|---|---|
| Cr | Provides corrosion resistance, oxidation resistance |
[Inconel 600 Chemical Composition (%)]
| Ni | Cr | Fe | C |
|---|---|---|---|
| 70.83 ~ 80.00 | 14.00 ~ 17.00 | 6.00 ~ 10.00 | Max. 0.15 |
| Cu | Si | Mn | S |
|---|---|---|---|
| Max. 0.50 | Max. 0.50 | Max. 1.00 | Max. 0.02 |
[Inconel 600 Mechanical Properties]
| Tensile Strength (Mpa) | Yield Strength (Mpa) | Elongation (%) |
|---|---|---|
| 585 | 240 | 30 |
[Inconel 600 Physical Properties]
| Density (g/㎤) | Melting Range (℃) | Specific Heat (0-100℃), J/kg*℃ | Curie Temperature (℃) |
|---|---|---|---|
| 8.47 | 1354 ~ 1413 | 444 | -124 |
3. Standard & Specification
– Specification : UNS N06600
| Product Form | ASTM | ASME | SAE | DIN |
|---|---|---|---|---|
| Bar, Rod | B166, B564 | SB166, SB564, N-253 | AMS 5665, AMS 5687 | 17752 |
| Plate, Sheet, Strip | B168, B906 | SB168, SB906, N-253 | AMS 5540 | 17750 |
| Wire | B166 | – | – | – |
| Pipe, Tube | B167, B163, B516, B517 | SB167, SB163, SB516, SB517, SB751, SB775, SB829, N-20, N-253, N-576 | AMS 5580 | 17751 |
| Forgings | B366 | – | – | – |
4. Available Form
– Bar, Rod
– Sheet, Plate, Strip
– Pipe, Tube
– Forgings
– Wire
5. Application & Product
– Aerospace, Chemical, Electronics
| Application | Product |
|---|---|
| Aerospace | Exhaust liners, turbine seals, engines, airframe components, combustion can liners |
| Chemical | Distillers, condensers, heat exchangers, condensing tubes |
| Electronics | Cathode Ray Tubes |

(1) Turbine seals / (2) Combustion can liners / (3) Heat exchangers / (4) Cathode ray tubes