1. Introduce
– Ni-Cr alloy with high Cr content and some Al, which provides excellent resistance to high temperature oxidation and corrosion
– Excellent oxidation resistance and high temperature material properties up to a temperature range of 1250℃
– High temperature mechanical properties superior to Inconel 600 due to increased Cr and Al content
– UNS N06601
* Inconel
- Features
– Resists oxidation and submersion in oxidizing and sulfurizing atmospheres above 900℃
– Non-corrosive to organic and salt solutions
– Excellent mechanical properties such as tensile and yield strength up to about 600℃ - Applications
– High temperature heat resistant equipment(Heat treatment furnace, boiler, jet engine parts, electric heater parts) - Types
– Incoenl 600/601, Inconel 625, Inconel 690, Inconel 718, Inconel 718+, Inconel X-750, etc.
* UNS
- Abbreviation for Unified Numbering Systems for Metals and Alloys
- Unified unique numbering system for metals and alloys
- A representative number that is compatible with metals and alloys defined in many material-related codes such as ASTM, AISI, ASME, AWS, etc.
* N : Nickel and Nickel Alloys
* UNS N06601 : 06XXX : Chromium(Hastelloy, Nichrome, Inconel and etonite, some with additional element
2. Property
– Heat resistance, corrosion resistance, electrical resistance, high temperature oxidation resistance, formability, good machinability
| Element | Impact |
|---|---|
| Cr | Provides corrosion resistance, oxidation resistance |
| Al | Component of γ’, the main strengthening phase of nickel-based super heat-resistant alloys, provides high temperature creep characteristics, oxidation resistance |
[Inconel 601 Chemical Composition (%)]
| Ni | Cr | Fe | C | Al |
|---|---|---|---|---|
| 58.00 ~ 63.00 | 21.00 ~ 25.00 | 7.68 ~ 20.00 | Max. 0.10 | 1.00 ~ 1.70 |
| Cu | Si | Mn | S | |
|---|---|---|---|---|
| Max. 1.00 | Max. 0.50 | Max. 1.00 | Max. 0.02 |
[Inconel 601 Mechanical Properties]
| Tensile Strength (Mpa) | Yield Strength (Mpa) | Elongation (%) |
|---|---|---|
| 690 | 372 | 42 |
[Inconel 601 Physical Properties]
| Density (g/㎤) | Melting Range (℃) | Specific Heat (0-100℃), J/kg*℃ | Curie Temperature (℃) |
|---|---|---|---|
| 8.11 | 1360 ~ 1411 | 448 | <-196 |
3. Standard & Specification
– Specification : UNS N06601
| Product Form | ASTM | ASME | DIN | EN |
|---|---|---|---|---|
| Bar, Rod | B166 | SB166 | 17752 | 10095 |
| Plate, Strip, Sheet | B168 | SB168 | 17750 | 10095 |
| Wire | B166 | SB166 | 17753 | – |
| Pipe, Tube | B775, B829, B167, B751 | B167, SB751, SB775, SB829 | 17751 | – |
| Forgings | B166 | – | 17754 | – |
4. Available Form
– Bar, Rod
– Plate, Strip, Sheet
– Wire
– Pipe, Tube
– Forgings
5. Application & Product
– Marine, Chemical, Aerospace
| Application | Product |
|---|---|
| Marine | Propeller shaft, Fasteners |
| Chemical | Process vessels, Valves, Heat exchangers, Boiler feed water heaters |
| Aerospace | Turbine engine igniters, Combustion can liners, Diffuser assemblies |

(1) Marine propeller shaft / (2) Boiler feed water heater / (3) Turbine engine igniter / (4) Diffuser assembly