1. Introduce
– Highly strengthened Ni-Cr-Co-Mo alloy with excellent high temperature strength and oxidation resistance properties
– Excellent high strength and oxidation resistance properties up to a temperature range of 980°C
– Has similar high temperature resistance properties to Inconel 600 and 601 with improved strength and corrosion resistance similar to Inconel 625
– UNS N06617
* Inconel
- Features
– Resists oxidation and submersion in oxidizing and sulfurizing atmospheres above 900℃
– Non-corrosive to organic and salt solutions
– Excellent mechanical properties such as tensile and yield strength up to about 600℃ - Applications
– High temperature heat resistant equipment(Heat treatment furnace, boiler, jet engine parts, electric heater parts) - Types
– Incoenl 600/601, Inconel 625, Inconel 690, Inconel 718, Inconel 718+, Inconel X-750, etc.
* UNS
- Abbreviation for Unified Numbering Systems for Metals and Alloys
- Unified unique numbering system for metals and alloys
- A representative number that is compatible with metals and alloys defined in many material-related codes such as ASTM, AISI, ASME, AWS, etc.
* N : Nickel and Nickel Alloys
* UNS N06617 : 06XXX : Chromium(Hastelloy, Nichrome, Inconel and etonite, some with additional element
2. Property
– High temperature strength, creep resistance, oxidation resistance, good corrosion resistance
| Element | Impact |
|---|---|
| Cr | Provides corrosion resistance, reduction and oxidation resistance |
| Co | Highly strengthening element, provides strength and creep properties |
| Mo | Highly strengthening element, provides high temperature creep properties |
| Al | Component of γ’, the main strengthening phase of nickel-based super heat-resistant alloys, provides high temperature creep properties and oxidation resistance |
[Inconel 617 Chemical Composition (%)]
| Ni | Cr | Fe | C | Al |
|---|---|---|---|---|
| 43.22 ~ 61.15 | 20.00 ~ 24.00 | Max. 3.00 | 0.05 ~ 0.15 | 0.80 ~ 1.50 |
| Ti | Cu | Si | Mn | Mo |
|---|---|---|---|---|
| Max. 0.60 | Max. 0.50 | Max. 1.00 | Max. 1.00 | 8.00 ~ 10.00 |
| S | Co | B | ||
|---|---|---|---|---|
| Max. 0.02 | 10.00 ~ 15.00 | Max. 0.01 |
[Inconel 617 Mechanical Properties]
| Tensile Strength (Mpa) | Yield Strength (Mpa) | Elongation (%) |
|---|---|---|
| 710 | 340 | 62 |
[Inconel 617 Physical Properties]
| Density (g/㎤) | Melting Range (℃) | Specific Heat (0-100℃), J/kg*℃ |
|---|---|---|
| 8.36 | 1332 ~ 1380 | 419 |
3. Standard & Specification
– Specification : UNS N06617
| Product Form | ASTM | ASME | SAE | DIN |
|---|---|---|---|---|
| Bar, Rod | B166 | SB166 | AMS 5887 | 17752 |
| Plate, Sheet, Strip | B168 | SB168 | AMS 5888, AMS 5889 | 17750 |
| Pipe, Tube | B546 | SB546 | – | 17751 |
| Wire | B166 | SB166 | – | 17753 |
| Forgings | – | – | – | 17754 |
4. Available Form
– Bar, Rod
– Plate, Sheet, Strip
– Pipe, Tube
– Wire
– Forgings
5. Application & Product
– Aerospace, Chemical
| Application | Product |
|---|---|
| Aerospace | Gas turbines, Exhaust ducts, Combustion cans, Transition liners |
| Chemical | Heat exchangers in ultra-high temperature gas cooling furnaces for hydrogen production, High temperature gas pipes, High temperature piping |

(1) Gas turbines / (2) Exhaust ducts / (3) High-temperature piping


Leave a Reply