1. Introduce
– Nickel-based solid solution superalloy with a Ni-Cr base strengthened by the addition of Nb/Mo solid solution strengthening elements
– Excellent strength and toughness at about 980℃ and good oxidation and corrosion resistance
– Excellent ductility and toughness at about -196°C
→ Solid solution strengthening effect of refractory metals Nb, Mo in Ni-Cr base
– UNS N06625
* Inconel
- Features
– Resists oxidation and submersion in oxidizing and sulfurizing atmospheres above 900℃
– Non-corrosive to organic and salt solutions
– Excellent mechanical properties such as tensile and yield strength up to about 600℃ - Applications
– High temperature heat resistant equipment(Heat treatment furnace, boiler, jet engine parts, electric heater parts) - Types
– Incoenl 600/601, Inconel 625, Inconel 690, Inconel 718, Inconel 718+, Inconel X-750, etc.
* UNS
- Abbreviation for Unified Numbering Systems for Metals and Alloys
- Unified unique numbering system for metals and alloys
- A representative number that is compatible with metals and alloys defined in many material-related codes such as ASTM, AISI, ASME, AWS, etc.
* N : Nickel and Nickel Alloys
* UNS N06625 : 06XXX : Chromium(Hastelloy, Nichrome, Inconel and etonite, some with additional element)
2. Property
– Good high temperature strength, creep resistance, corrosion resistance, oxidation resistance, fatigue strength, stress corrosion cracking resistance
– Good machinability and weldability, no susceptibility to cracking after welding
| Element | Impact |
|---|---|
| Cr | Provides corrosion resistance, oxidation resistance |
| Mo | Highly reinforced element, high temperature oxidation resistance, cryogenic oxidation resistance, weldability |
| Nb | Highly strengthened element, provides strength |
| Ta | Highly strengthened, provides enhanced creep resistance, heat resistance, corrosion resistance |
[Inconel 625 Chemical Composition (%)]
| Ni | Cr | Fe | C | Al |
|---|---|---|---|---|
| 54.91 ~ 68.85 | 20.00 ~ 23.00 | Max. 5.00 | Max. 0.10 | Max. 0.40 |
| Ti | Si | Mn | Mo | S |
|---|---|---|---|---|
| Max. 0.40 | Max. 0.50 | Max. 0.50 | 8.00 ~ 10.00 | Max. 0.02 |
| Co | Nb | P | ||
|---|---|---|---|---|
| Max. 1.00 | 3.15 ~ 4.15 | Max. 0.02 |
[Inconel 625 Mechanical Composition]
| Tensile Strength (Mpa) | Yield Strength (Mpa) | Elongation (%) |
|---|---|---|
| 724 ~ 1104 | 290 ~ 759 | 30 ~ 65 |
[Inconel 625 Physical Properties]
| Density (g/㎤) | Melting Range (℃) | Specific Heat (0-100℃), J/kg*℃ | Curie Temperature (℃) |
|---|---|---|---|
| 8.44 | 1290 ~ 1350 | 402 | -196 |
3. Standard & Specification
– Specification : UNS N06625
| Product Form | ASTM | SAE | AWS |
|---|---|---|---|
| Bar, Rod | B166, B446 | – | – |
| Plate, Sheet, Strip | B168, B906, B443 | – | – |
| Tube, Pipe | B444, B167, B829, B517, B775, B516, B751, B704, B705 | AMS 5581 | – |
| Wire | B166, B446 | – | A5.14 ERNiCrMo-3 |
| Fittings | B366 | – | – |
| Forgings | B472, B564 | – | – |
4. Available Form
– Bar, Rod
– Plate, Sheet, Strip
– Wire, Weld Rod
– Forgings
– Tube, Pipe
5. Application & Product
– Aerospace, Desulfurization, Chemical, Marine
| Application | Product |
|---|---|
| Aerospace | Rocket engine combustion chamber tubes, Compressor vanes, Turbine seals, Thrust chamber piping for rockets, Aero engines |
| Desulfurization | Absorption towers, Reheaters, Exhaust gas inlet barriers, Fans (moisture), Agitators, Deflectors |
| Chemical | Piping, Valves, Reactors, Heat exchangers, Tubing for heat exchangers |
| Marine | Submarine communication cables, Exhaust ducts for submarines and boats, Bellows for underwater control devices |

(1) Turbine seals / (2) Heat exchangers / (3) Submarine communication cables